Caesar Diamonds

Jewellery Quality Control at Every Stage

Quality control in jewellery making is a multi-point inspection at each stage, not a single check at the end. Castings are checked for porosity and shrinkage, settings for seat depth and security, finishes for surface and edge, and the finished piece for weight and hallmark before it is packed.

Checks at each stage, not one at the end

A fault found at the bench costs minutes to fix. The same fault found after setting and polishing costs a stone, a setting and a finish, and sometimes the whole piece. That is the practical argument for inspecting at every stage rather than once at the end.

The sequence is: the CAD model against the real stone, the casting against the model, the setting against the stone, the finished surface against the approved finish, and the completed piece against the metal issued to the job.

Porosity and shrinkage in casting

Two faults are specific to casting. Porosity is trapped gas or shrinkage voids inside the metal, which shows as pits that appear when the surface is polished back. Shrinkage happens as the metal cools and contracts, and it pulls a casting slightly away from the model's dimensions.

Both are managed by how the casting is fed and cooled, not by polishing harder afterwards. A porous casting will keep revealing pits as it is finished, so the inspection happens before the setter sees it. Where a casting cannot be saved, it is recast rather than patched, because a patch in a thin section will fail in wear.

Assay at a UK assay office

Hallmarking is carried out by one of the UK assay offices, and only an assay office may apply a hallmark. The workshop submits the finished piece, the office tests the metal and strikes the marks, and the piece comes back with the record attached to the job.

Assay adds 3-5 working days. The three compulsory marks are the assay office mark, the metal fineness mark and the maker's mark. There are exemption weights below which a hallmark is not compulsory: silver 7.78g, gold 1g, palladium 1g and platinum 0.5g.

The GIA report number against the job

Where a diamond carries a GIA grading report, the report number is recorded against the job rather than filed separately. That single field is what lets the finished piece, the certificate and the project record line up years later, when a customer asks about the stone.

For parcels and melee, the parcel description and grade are recorded instead, so it is clear what was supplied even where individual reports do not exist.

What the documentation pack contains

At the end of a job the record holds the approved CAD render, the metal specification and the weight issued, the stone specification with certificate numbers, the inspection notes from each stage, production photography, and the hallmark record. Remodelling and repair jobs also hold a condition report on the stones as received.

That pack is not paperwork for its own sake. It is what allows a question two years later, about a stone, a finish or a resize, to be answered from evidence rather than recollection.

At a glance

Specification and turnaround for this service
Typical turnaroundInspection runs alongside the standard 2-4 week build. Assay adds 3-5 working days.
Metals18k white, yellow and rose gold, platinum, palladium and silver.
Stones we setEvery stone is checked for seat depth, security and alignment before the piece is finished.
What you supplyThe brief or specification, and any certificate you already hold for a stone.
What you get backThe finished piece plus the documentation pack: renders, certificate numbers, inspection notes, photography and hallmark record.
Where it happens100 Hatton Garden, Suite 225, London EC1N 8NX, with assay at a UK assay office.

Frequently Asked Questions

What is porosity in a casting?

Trapped gas or shrinkage voids inside the metal, which appear as pits when the surface is polished back. It is controlled by how the casting is fed and cooled, not by polishing harder. A casting that cannot be saved is recast rather than patched.

Why does casting shrink?

Metal contracts as it cools, so a casting comes out slightly smaller than the model. The shrinkage is predictable and is allowed for in the model, but uneven cooling can pull one section more than another, which is why the casting is measured against the model before setting.

Which marks are compulsory on a hallmark?

Three: the assay office mark, the metal fineness mark and the maker's mark. Only an assay office may apply a hallmark, and assay adds 3-5 working days to a build.

At what weight is a hallmark not required?

The exemption weights are silver 7.78g, gold 1g, palladium 1g and platinum 0.5g. Below those weights a hallmark is not compulsory. Above them, it is required by the Hallmarking Act 1973.

What is in the documentation pack?

The approved render, the metal specification and weight issued, the stone specification with certificate numbers, inspection notes from each stage, production photography and the hallmark record. Remodels and repairs also hold a condition report on the stones as received.

Talk it through

Send a brief, a sketch or a photograph, or book an hour at 100 Hatton Garden, Suite 225, London EC1N 8NX. We will confirm what is possible, the timeline and a written quote before any work starts.

Contact the workshop
Chat with us

We Value Your Privacy